Material consumption: 0.25 mg/h when the intensity of 40Ca11+ of 30 µA was produced.
Note 1: At JYFL CaO powder is mixed with Zr powder and then a pellet is pressed.
...
...
Material consumption: 0.25 mg/h when the intensity of 40Ca11+ of 30 µA was produced.
Note 1: At JYFL CaO powder is mixed with Zr powder and then a pellet is pressed.
...